Initial investigations of investment cast superalloy lattice block suggest that this technology will yield a low cost approach to utilize the high temperature strength and environmental resistance of superalloys in lightweight, damage tolerant structural configurations. Work to date has demonstrated that relatively large superalloy lattice block panels can be successfully investment cast from both IN-718 an ... Täielik kirjeldus

Võib-olla meeldib sulle ka

Kirjeldus

Initial investigations of investment cast superalloy lattice block suggest that this technology will yield a low cost approach to utilize the high temperature strength and environmental resistance of superalloys in lightweight, damage tolerant structural configurations. Work to date has demonstrated that relatively large superalloy lattice block panels can be successfully investment cast from both IN-718 and Mar-M247. These castings exhibited mechanical properties consistent with the strength of the same superalloys measured from more conventional castings. The lattice block structure also accommodates significant deformation without failure, and is defect tolerant in fatigue. The potential of lattice block structures opens new opportunities for the use of superalloys in future generations of aircraft applications that demand strength and environmental resistance at elevated temperatures along with low weight.

Lisateave

Autor M. V. Nathal, Nasa Technical Reports Server (Ntrs), Et Al
Kirjastaja BiblioLife
Väljalaskeaasta 2013
Kaanetüüp Pehme kaanega
EAN 9781289146191
Kirjuta oma arvustus
Te vaatate: Superalloy Lattice Block Structures
Teie hinnang:

Goodreads'i arvustused

19,31 € 32,18 €